Injection Molding InsightsPractical injection molding knowledge for buyers and engineers.
Process & Defects

How to Set Cooling Time for Thick-Walled Parts

Published 7 min read

Cross-section view of a plastic part with visible internal cooling channels
Quick answer

To set cooling time for thick sections, identify the material and mold geometry, calculate the solidification window, and verify the result through in-mold temperature checks and part testing. A structured approach prevents sink marks and warpage while maintaining press efficiency.

Key takeaways
  • Start with the material-specific solidification time, not a generic rule of thumb.
  • Use the mold geometry and thermal mass to adjust the calculated window.
  • Verify with in-mold temperature sensors and part inspection before locking the recipe.
  • Treat cooling time as a balance between dimensional stability and press throughput.

Why Thick Walls Change the Cooling Equation

Thick-walled parts behave differently from thin-walled shells. The material in the center of a 6 mm or 8 mm wall does not see the mold surface temperature immediately. Heat must conduct from the hot melt to the mold steel, and the cooling time must account for that conduction path. If you set the cooling duration based only on thin-wall experience, the part leaves the mold with a semi-liquid core. That core continues to shrink in the mold cavity and creates sink marks, short shots, or warped parts after demolding.

The goal is to find the shortest cooling time where the part is dimensionally stable and free of internal stress, without dragging the cycle time so far that press utilization drops. This is a thermal management problem, not a guessing game.

What You Need Before Calculating Cooling Time

Before you touch the machine parameters, gather the following inputs.

  • Material grade and melt flow index. Higher melt flow indices cool slightly faster but also carry more internal stress.
  • Part wall thickness at the thickest section. Use the maximum thickness, not the average.
  • Mold steel type and cooling channel geometry. Aluminum molds cool faster than steel molds. Circular channels cool faster than serpentine or conical channels.
  • Mold temperature settings. The mold steel temperature directly changes the heat transfer rate.
  • Injection parameters. Higher injection pressure can increase pack-out behavior, which modifies the effective cooling window.

If you do not have the mold steel type or channel layout, you are working without the two variables that most affect heat extraction. Ask the mold maker for the drawing or the thermal model output. Do not proceed with a blank assumption.

Step 1: Identify the Material-Specific Solidification Window

Every material has a temperature range where it transitions from a viscous melt to a solid. For engineering thermoplastics like ABS, PC, or PA, this transition happens at different temperatures than for commodity grades like PP or HDPE. Use the material supplier’s technical data sheet to find the glass transition temperature, or Tg, and the melting range.

The solidification window for a thick wall is the time required for the core to drop below the Tg. Once the core is below Tg, the polymer chains are locked in place and further shrinkage is minimal. This is the baseline. If your core temperature remains above Tg after the cooling phase, the part will continue to shrink during the next few seconds or minutes. That residual shrinkage is what you see as warpage.

For a quick estimate, use the material’s thermal conductivity and specific heat capacity. If the supplier does not provide these values, ask a process engineer. Do not rely on a generic chart that lumps all thermoplastics together.

Step 2: Determine the Mold Geometry and Cooling Channel Layout

The mold geometry dictates how much of the part surface is in contact with the cooling channels. A flat wall with a single circular channel behind it cools differently than a ribbed section with multiple serpentine channels. The key variable is the thermal resistance between the melt and the channel water.

Map the thickest section of the part. Identify where the cooling channels are closest to that section. If the channel is more than 10 mm away from the part surface, the conduction path is longer and the cooling time must increase. If the channel is directly behind the thickest wall, the heat extraction is faster, but the channel itself must have enough surface area to absorb the heat without overheating.

Check the channel diameter and water flow rate. A 6 mm channel with low flow will create a hot spot at the channel centerline. That hot spot delays cooling of the adjacent part area. If the channel layout is not optimized, you may need to increase the cooling time to compensate for the slowest-cooling region, not the average.

Step 3: Calculate the Baseline Cooling Duration

Use the solidification window from Step 1 and the thermal resistance from Step 2 to estimate the cooling duration. A practical method is to measure the in-mold temperature at the thickest section using a thermocouple or an IR sensor mounted in the mold.

Start with a conservative estimate. Set the cooling time to a value that allows the core temperature to drop at least 10 degrees below the Tg. Run the injection cycle and record the time it takes for the sensor to reach that temperature. This measured time is your baseline.

Do not rely on a fixed rule such as one second per millimeter of thickness. That rule works for thin walls in simple molds, but it fails for thick sections with complex cooling. The measured time accounts for the actual heat transfer in your specific mold.

Step 4: Adjust for Mold Steel and Water Temperature

The mold steel type and the cooling water temperature both change the heat transfer rate. Aluminum molds have higher thermal conductivity than steel molds, so the same part cools faster in aluminum. Steel molds retain more heat and require longer cooling times.

Cooling water temperature matters more than most operators realize. If the water enters the mold at 25 degrees Celsius and the part core is at 200 degrees, the temperature gradient is large and heat is extracted quickly. If the water is preheated to 60 degrees, the gradient is smaller and cooling is slower. For most engineering plastics, keep the cooling water between 40 and 60 degrees to balance speed and mold wear. For high-heat-build materials, lower the water temperature to 30 to 45 degrees to accelerate heat extraction.

Adjust your baseline cooling time by the water temperature differential. If you increase the water temperature by 10 degrees, expect the cooling time to increase by a measurable amount. Measure it. Do not guess.

Step 5: Factor in Pack-Out and Hold Pressure

Thick-walled parts often require pack-out to compensate for shrinkage during solidification. The hold pressure pushes additional melt into the part as it cools. This pack-out phase changes the effective cooling time because the part continues to receive material while the outer layers are solidifying.

If the hold pressure is too high, it can create internal stress and residual warpage. If it is too low, the part will shrink and create sink marks. The cooling time must be long enough to allow the hold phase to finish without the outer surface cracking or the core remaining liquid.

Run the cycle with the hold pressure set to the recommended value. Record the time from the end of injection to the start of cooling. If the hold phase extends into the cooling window, add that duration to your cooling calculation.

Step 6: Verify with In-Mold Temperature and Part Inspection

The final verification step is non-negotiable. Measure the core temperature of the part at the moment of demolding. If the core is above the Tg, increase the cooling time. If the core is well below the Tg, you may be able to reduce the cooling time and improve throughput.

Inspect the part for sink marks, short shots, and warpage. Sink marks on the thickest section indicate insufficient cooling or insufficient pack-out. Warpage indicates that the part cooled unevenly or that the core remained above Tg during demolding.

Use a caliper to measure the critical dimensions. If the dimensions are out of tolerance, adjust the cooling time and re-measure. A small change in cooling time can shift the dimensional stability by a few thousandths of an inch.

Common Mistakes That Ruin Cooling Settings

The most common mistake is using a generic rule of thumb without measuring the actual heat transfer. Another is ignoring the cooling channel layout. If the channels are not evenly spaced, the part cools unevenly, and the slowest-cooling region dictates the cycle time.

Operators also make the mistake of setting the cooling time too long. Excessive cooling time increases the cycle time without improving part quality. The part is already solid, and the extra time only delays demolding.

A third mistake is not checking the cooling water flow. If the flow is too low, the channel overheats and the part cools slower than expected. This creates a false impression that the cooling time needs to be increased, when the real problem is insufficient water flow.

Final Verification and Lock-In

Once you have the baseline cooling time, adjust for water temperature, pack-out, and part inspection results, you have a working recipe. Lock in the parameters and run a short production run to confirm stability.

Record the cycle time, the core temperature at demolding, and the part dimensions. If all three are within tolerance, the cooling time is set. If any parameter drifts, return to the verification step and adjust.

Cooling time is not a single value. It is a balance between material solidification, mold heat transfer, and part quality. Measure it, adjust it, and verify it. Do not rely on assumption.

Quick Reference Table

Parameter Typical Range Effect on Cooling Time
Wall thickness 4 mm to 10 mm Longer walls require longer cooling
Mold steel Aluminum or steel Steel requires longer cooling than aluminum
Water temperature 30 to 60 degrees Celsius Higher water temperature increases cooling time
Channel spacing 6 mm to 12 mm Wider spacing increases cooling time
Hold pressure Material dependent Longer hold adds to effective cooling window

Final Check

Before releasing the part to production, confirm the following. The core temperature at demolding is below the Tg. The part dimensions are within tolerance. The sink marks are absent or below the visual acceptance level. The cycle time is stable across ten consecutive shots. If all four checks pass, the cooling time is set.

Frequently asked questions

What is the typical cooling time for a 6 mm thick ABS part?

It depends on the mold steel, channel layout, and water temperature. Measure the in-mold temperature and adjust until the core is below the Tg.

Can I reduce cooling time if I increase the injection pressure?

Higher injection pressure can increase pack-out, but it does not accelerate cooling. Cooling time is controlled by heat transfer, not melt pressure.

How do I know if the part is fully solid before demolding?

Check the core temperature with an in-mold sensor. If the core is below the Tg, the part is solid and should be dimensionally stable.

Does the cooling water flow rate affect the cooling time?

Yes. Low flow rate creates hot spots in the channel, which slow heat extraction. Increase the flow rate to reduce cooling time.

What happens if I set the cooling time too short?

The part may leave the mold with a semi-liquid core, leading to sink marks, short shots, or warpage after demolding.